  1. Hi Devorka, your work is fantastic! Tell me did you manage to put a website together yet? Jacqui

  2. Hi there, wishing you all the best with your ceramic art journey. If you put your mind to it you can go far with ceramics, it is a long journey and one must remember to be patient. I also recommend getting some books and dropping into ceramic artists studios. All the best! Jacqui

  3. Hi there, no I don't mind input about Numerology, I find it all quite interesting, so if you have any other information, I would be most intrigued. About your cracked bottoms on your pots. I have a feeling this is due to too much use of water when joining. When I work with slabs, and score my slabs on both surface areas I then use a slip , which I make up as a paste from the clay I'm wo...

×
×