I'd love to hear what you learned. It's unlikely I'll have the opportunity to build a reduction electric kiln in the near future, but I'm still interested.
-
From the album: Glaze tests
-
From the album: Glaze tests
-
From the album: Glaze tests
-
From the album: Glaze tests
-
From the album: Glaze tests
-
From the album: Glaze tests
-
Seger cone 4 + RIO
Pieter Mostert commented on Pieter Mostert's gallery image in Browse Member Galleries
-
Seger cone 4 + RIO
Pieter Mostert commented on Pieter Mostert's gallery image in Browse Member Galleries
-
From the album: Glaze tests
Fluxing effect of iron oxide in oxidation. -
From the album: Glaze tests
Work in progress. Alumina increases as you go up. Left column replaces some magnesium in the right column with calcium. -
From the album: Glaze tests
Varying alumina and iron in a spotty glaze. Test on white stoneware. -
From the album: Glaze tests
Detail of test on red earthenware. -
From the album: Glaze tests
Varying alumina and iron in a spotty glaze. Test on red earthenware. -
This is just calcined Colemanite in some water in a polystyrene cup. See my post in this thread for more context: http://community.ceramicartsdaily.org/topic/15955-colemanite/ I think the lighter coloured bits floating on the water are thin layers of soluble material that have crystallised. You can also see a ring of white crystals above the water line.
-
Calcined Colemanite
Images added to a gallery album owned by Pieter Mostert in Browse Member Galleries
-
From the album: Calcined Colemanite
-
From the album: Calcined Colemanite
-
From the album: Calcined Colemanite
-