Did a Raku firing last night with some test tiles for my Art Club firing this week. Also used a pumpkin as a reduction chamber for a ceramic pumpkin... Yes, clever I know...
- Show previous comments 1 more
-
''Tis the season
-
''Tis the season
-
Babs, I tried something similar a couple years ago, but scooped out the "guts" first, and dried the pumpkin a bit. Some interesting results. This time, I just cut the top off the pumpkin, and put the hot ware directly into the pumpkin guts, seeds and all. The pumpkin top seals nicely to keep the air out. Pretty interesting result. I'll post photos later.