Glaze firing on - mostly transparent over oxides and tissue transfers with my v reliable glossy glaze. On the shelf is a batch of stoneware pieces from a throwing workshop I attended - after 2 failed stoneware glaze firings I'm very reluctant to get on with these. Have tweaked the glaze and will do just one test piece before sacrificingthe rest to the kiln gods
- Show previous comments 2 more
-
Will post pics in the morning when I unload.
That's a very good question Roberta - it crawled horribly on various pieces. I THINK I'd thinned it too much with water, when someone suggested it should be thin (after a precious disaster!). Now, I've drawn off the excess water and will be programming a slow cool. Problem is getting enough stoneware together to fill the kiln and having the right pieces for a different glaze to accompany my test piece.
-
That was - 'previous' disaster - though the work was of course 'precious' !!!!
-
Pictures in my gallery. Quite pleased - some glaze a bit thin and oxides on the pale side. I was trying not to overload either! Cobalt transfers on the creamers have run a little at this temp, so will fire lower next time. Full speed ahead for the rest of the wedding favours, now I know the glaze will work.