  1. Hi Laura,

    I have never had a problem firing my sculptures. I do however let the work dry five weeks before I even consider firing. Five weeks is not a magic number it just seems to work well for me. I then fire on low (vented), continue on medium (closed kiln) and finish on high to cone 05. The entire process takes about ten hours. I can give you my entire proceedure if you like but Chris and Paul are correct, the work is not dry enough.

×
×