glazenerd 1,807 Posted April 5, 2018 Report Share Obviously cobalt, but adding tin perhaps? Quote Link to comment
1515art 260 Posted April 7, 2018 Report Share No, no tin just cobalt oxide with water and dish soap experiment over a mix of coyote cone 6 glaze under the oxide and finished with a low fire clear third fire. Quote Link to comment
1515art 260 Posted April 7, 2018 Report Share I did splash some additional cobalt and iron oxide on the lower third but you can't really see that in the picture. Quote Link to comment
glazenerd 1,807 Posted April 7, 2018 Report Share I have a crystalline recipe that uses cobalt and tin; plus a dash of rare earth oxide. The end result is similar to yours. Quote Link to comment
1515art 260 Posted April 9, 2018 Report Share Nerd, have you posted pics of that crystalline glaze? Quote Link to comment