Dawn Ferguson Platter
Cone 6 porcelain, underglaze and transparent colored overglaze
Photo Information
- Taken with NIKON CORPORATION NIKON D3200
- Focal Length 18 mm
- Exposure Time 1/125
- f Aperture f/5.6
- ISO Speed 360
Cone 6 porcelain, underglaze and transparent colored overglaze