Jump to content
Parian Vase
 
© Christine Cherry Ceramics

chezzi64
 Share


This is a vase I made out of Parian Porcelain.It is slip-cast then carefully finished. It is fired to 1200 C with a 45 minute soak, this vitrifies the clay body so that no glaze is needed. I then polish the vessel, resulting in a beautifully smooth, translucent vase.

Copyright

© Christine Cherry Ceramics
From the album:

My work 2017 (Year 1)

  • 8 images
  • 0 comments
  • 9 image comments

 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.