Jump to content

Progressive Talc Additions in Stoneware Clay Body


curt

Here are five very similar clay bodies fired in both oxidation and reduction at cone 10. Talc is increasing progressively from bottom to top and if you look carefully this seems to be imparting a gray or dark color to the clay in both types of firings.

From the album:

Talc Testing

· 6 images
  • 6 images
  • 0 comments
  • 3 image comments

Photo Information

  • Taken with Apple iPhone 6 Plus
  • Focal Length 4.2 mm
  • Exposure Time 1/179
  • f Aperture f/2.2
  • ISO Speed 32

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.