alabama 155 Posted April 7, 2016 Report Share If the vertical cracks bother you, try adding a coil of clay with 37% quartz sand wedged in to it. If that doesn't work or change the direction of the cracks, add 42% sand by volumn to the entire unit of clay. Then respond to the results to make any corrections. Just saying! Quote Link to comment