Tennis Net Mugs - Handle Finial Detail
These two mugs are a hybrid combination of hand-built and wheel-thrown construction. The rim is the only wheel-thrown piece and is included only because I have never been quite satisfied with my efforts to hand-build rims on mugs. Unique to the stamped-on, tennis net theme are the athletic shoe & tennis ball finials to the pulled handle. The mugs are 14oz-16-oz capacity stoneware, fired Cone 10 reduction. Interior glaze is Woo's Blue. Exterior is clear, sprayed on in two light coats.