A hand built stoneware box impressed with my InCOGneatoh Intaglio rubber stamp mat and finished with ocher terra sigillata.

Copyright

© BHClaysmith
From the album:

CLAY TO SHARE

  • 14 images
  • 0 comments
  • 7 image comments

Photo Information for Wishful Thinking Pyxis

Taken with SAMSUNG TECHWIN CO., LTD. Digimax A6

  • 8.1 mm
  • 1/78
  • f f/2.7
  • ISO 50
View all photo EXIF information
 Share


Recommended Comments

Here are the recipes for two really nice ocher terra sigillata mixes.  Since Albany Slip is no longer available, you can make the Weiser Ocher one instead which is just as nice!

 

ALBANY SIG

50 grams Albany slip

50 grams KYOM4

400 grams water

10 grams Sodium Hexametaphosphate

 

OCHRE SIG by Weiser

1663 grams Cedar Heights Gold Art

66 grams Yellow Ochre

 

Add to a mixture of:

8 grams soda ash

16 grams Sodium Hexametaphosphate

1 gallon water

Link to comment

Sodium Hexametaphosphate is the original "Calgon" formula plus perfume which was made in the US awhile back. It was reformulated due to the adverse effect the chemical had on the the microscopic flora in streams and rivers but can still be purchased from certain chemical supply houses. I believe it is used by people involved with pool cleaning.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.