Dancing Away
White clay and the same clay with iron oxide wedged into it. The piece was dunked in glaze and then scraped away leaving a pronounced coil texture.
∆6 oxidation
Copyright
© Matthew Van Atta
White clay and the same clay with iron oxide wedged into it. The piece was dunked in glaze and then scraped away leaving a pronounced coil texture.
∆6 oxidation