SydneyGee 63 Posted September 6, 2016 Report Share What glaze(s), cone temp, and clay is this? I love it! Quote Link to comment
AndreaB 67 Posted September 7, 2016 Report Share Hi Sydney, thanks for the compliment. It's also one of my favs. I'm in South Africa so the glaze and stoneware are completely different to what you have. I threw a stoneware that fires to a light beige. Textured the pot and on glazing I used two glazes. The one I use as a base glaze with a lot of my textured pots, it's called lace and is a beige matt glaze. The other was applied first and then scraped off so that it lay within the texture. It wasn't comletey removed which causes the colours to bleed into each other. This sort of combination was also used in the mug. The stoneware was fired to cone 8 Quote Link to comment