Bowl with clear glaze with copper carbonate and cobalt blue wax resist design
Smalll bowl 7 inches in diameter with copper over transparent glase with wax resist and cobalt over that.
Copyright
© craig fulladosa
Smalll bowl 7 inches in diameter with copper over transparent glase with wax resist and cobalt over that.