Bisque Imports teapot
I don't know if you can tell from the photo but the teapot sort of "soaked in" the white glaze leaving a matte surface with tiny pinholes in it. Very awful. On the inside the delft blue had incomplete spots that were matte and a totally different color of blue. This was not fixed upon a second firing with another coat of clear, so my sister took it as a garlic storage pot since no food will be touching the incomplete surface.