Marko 191 Posted February 5, 2016 Report Share Wow! That's a setup. Love the bricks. Quote Link to comment
High Bridge Pottery 879 Posted February 5, 2016 Report Share Wow! That's a setup. Love the bricks. If only it worked! Fired twice and stalled out at 1000c. Not getting anywhere near enough oxygen. Looking into power burners now to solve that problem. Quote Link to comment