bowl Top
Earthenware bowl
Glaze of 50/50 by weight Cryolite and Nepheline Syenite
Fired to 1050C with 15min soak
Photo Information
- Taken with Canon Canon PowerShot SX200 IS
- Focal Length 5 mm
- Exposure Time 10/10
- f Aperture f/8.0
- ISO Speed 80
Earthenware bowl
Glaze of 50/50 by weight Cryolite and Nepheline Syenite
Fired to 1050C with 15min soak
By using this site, you agree to our Terms of Use.