Sconce closeup image
This is made of ^6 Aardvark Clay's Bee Mix 5, Formed over a 6" PVC pipe. Slab rolled a 3/8" backing. cut hanging holes and a hole for the Xenon puck light. Assembled next day using Magic Water and some hand rolled clay for the joints. Next day, used a stencil to apply underglaze. Drilled light holes and fired ^6 ox.