basalt test. heavy reduction, cone 10. mostly still whole particles of what started as 40 mesh material. however, in spite of its appearance, this sample has fused together somehow internally and is not able to be removed from the test dish.

From the album:

ian currie test tiles

  • 27 images
  • 0 comments
  • 0 image comments

Photo Information for Basalt test

Taken with Apple iPhone 6 Plus

  • 4.2 mm
  • 1/746
  • f f/2.2
  • ISO 32
View all photo EXIF information

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.