this style was finished with Oribe green glaze sprayed pretty close to the leaf lines and a turquoise-ish blue on the other end. the green overspray was wiped off with a scrubby and the blue done secondly. the dragonfly is wiped with a tiny stiff brush to remove some of the overspray and then a loaded brushful of dark purple Mayco stroke&coat is touched to the deep impression. i only have one left after the mother's day sale.