020
bisque plate ready to pack. the seashells in relief are made from little loafers clay that was pressed into bisque molds made from actual shells. once they completely dry, putting them onto the completely dry dish is easy. decide where to put the clay shells and hold a fully water-loaded #3 brush just touching the top of each shell. water will run down the shell without disturbing the delicate pattern and firmly stick the shell to the plate. DO NO TOUCH OR DISTURB IT UNTIL THE NEXT DAY! the dryness of both the shell and the plate allows for multiple trial locations until you are satisfied.