a variety of shapes can touch each other in a bisque firing without causing problems. hanging over the edge of the shelf works too if there is firm support for the item. one inch posts allow stacking of the short things. for one and a half size posts, put a dab of glaze on the top of a 1 inch post and put a half inch post on top. fire together to cone 6 and you have a permanent 1 1/2 post. use a non-running glaze.