Embellished Blue Angel
This embellished angel was made with little loafers cone 6 clay. The designs were rolled into the surface and then glazed. The face was press molded with a minor hand sculpting. The hair was made with a mini extruder. The hair and face is painted with Amaco LUGs and the wings are coyote white and the dress is Coyote Opal.
This angel can be used as a stand alone figurine or it can be used as a tree topper. I added holes on either side so that it can be securely anchored to the tree.