blue Bird Utensil Holder
I made this utensil holder using little loafers cone 6 clay. The birds, vines and flowers are appliqués to give a 3 dimensional look to the surface. The design is painted with Amaco LUGs and then glazed in Amaco Zinc Free clear and the inside is Coyotes Rhubarb.