Dinah 7 Posted April 23, 2010 Report Share This is one of three slightly graduated in size Summer Teabowls for a series which I've submitted to the KC teabowl show juried by Pete Pinnell. This one is entitled Angles. I've rung the changes in the three with varying designs using strips of vintage OG transfers, but all have a gold luster wedge. Bowls sell for $35 @. Vashon white body bisqued to ^04, glazed to ^01, OG transfers and luster at ^016. Usually I fire lusters separately, but this time able to take advantage of the masking effect of the OG transfer. Quote Link to comment
BillPotter 0 Posted April 25, 2010 Report Share Dinah, I really like the simplicity of this piece. A few color strokes on a sea of white. Thank you. Bill Quote Link to comment