Porcelain loves to crack - sculpting porcelain is a fool's errand



Notice the 1/4" crack on the left side of my head, where the relief carving was a little thinner.

From the album:

Defects

  • 16 images
  • 0 comments
  • 0 image comments

Photo Information for Porcelain loves to crack - sculpting porcelain is a fool's errand

Taken with Panasonic DMC-TS2

  • 8.4 mm
  • 10/40
  • f f/4.5
  • ISO 500
View all photo EXIF information

Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.