Frederik-W 24 Posted November 27, 2013 Report Share I like the pose very much! Looks like an excited little duck! Quote Link to comment
Norm Stuart 82 Posted November 27, 2013 Report Share I tried to capture the look of photos of various ducks landing on water. This particular duck had to land in a pool with a wingspan no wider than our kiln, so he had to be captured at the moment he began tucking his wings back into a retracted position. I made it with Laguna WC-370 Amador clay which has so much grog it's almost like using paper-clay. The companion piece, Return of the Duck in Orange Sauce, is an assemblage of a variety of ^6 glazed clays and porcelain pieces assembled with low-fire glaze and low-fire glaze mixed with orange COE 96 glass frit. Quote Link to comment