Dark iron stoneware, wood fired and electric fired. Nuka glaze, gold luster, porcelain lid. In private collection in Japan.

Copyright

© &copy John Baymore all rights reserved

From the album:

John Baymore's Clay Work

· 31 images
  • 31 images
  • 0 comments
  • 39 image comments


Recommended Comments

John;

I came across a recipe for a Nuka glaze, which I understood to be white. I was interested in it as it uses wood ash, which I have an abundance of.[dangling participle there]. I mixed up a test. Like the surface quality, but it needs to be applied thicker. On your jar, are you putting it over black slip, or is it a black clay body? Looks beautiful.

Tom

Link to comment

Just saw this comment Tom.  Thanks.  Very dark clay body.... Sheffield #42 with added local granite dust.

Link to comment

Bumping this old conversation  - ran into it googling for some info on that Sheffield 42.  How's it for coiling do you think?  I only get my clay from Sheffield,  usually Elaine's  Porcelain,  but having hit 15" of woobly porcelain coil on a fat pot this morning  I'm thinking I want something sturdier with a different character and some color the for fairly thin, soft, larger organic coiled forms I want to try.   Thinking you might have  another idea if 42's not good for that - I have a gift cert there  and would prefer ^6-10. Any thoughts? (I've long admired your beautiful work, always takes my breath away!)

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.