this kiln is built with 8"density fiber 1" think. The hardware fiber, steel straps, nuts and bolts were all from hom depot along with airplane wire for the pullies. the pullies are from Wichita Falls Texas and are welded to angle iron welded to the support beams in the kiln shed. he counter weight is a bucket of rocks. This kiln is featured in Mel Jacobson 's book on 21st century kilns.

Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.