JohnnyK 895 Posted February 11, 2021 Report Share Am interesting, almost "crystalline" look, Marcia...what process did you use to accomplish the effect? Quote Link to comment
Marcia Selsor 1,981 Posted March 8, 2021 Report Share On 2/11/2021 at 8:09 AM, JohnnyK said: Am interesting, almost "crystalline" look, Marcia...what process did you use to accomplish the effect? I use cobalt sulphate for the base and calcium chloride flakes for the dots. Quote Link to comment
Hyn Patty 90 Posted April 26, 2022 Report Share This is a very lovely piece. Great job both on the form as well as the finish! Marcia Selsor 1 Quote Link to comment