Venicemud Posted December 30, 2013 Report Share Posted December 30, 2013 I have just opened a new (for me) bag of clay, Laguna B3 Brown. A little late in the day I decided to check the clay's characteristics and found that it has what seems to be a high COE - 7.25 x 10-6. Is this likely to create any problems when glazing? Mostly in the past I have used the Laguna cone 5 B mix and B mix with grog. Thanks for being there. Joan. Link to comment Share on other sites More sharing options...
Guest JBaymore Posted December 30, 2013 Report Share Posted December 30, 2013 Likely will cause crazing with glazes that fit the other low E clays. best, ....................john Link to comment Share on other sites More sharing options...