I was just wondering to what cone temperature it is best to bisque fire your raku pots to?



#2 Idaho Potter

Idaho Potter

    Learning all the time

  • Members
  • PipPipPip
  • 399 posts
  • LocationBoise, Idaho

Posted 25 September 2013 - 07:42 PM

Just fire as you would any bisque firing.  I use a raku clay with a firing range of cone 06 to cone 10, and never hope to achieve vitrification, so I bisque to 04 and raku glaze fire at 06. 

 

 

Shirley                            



#3 Benzine

Benzine

    Socratic Potter

  • Members
  • PipPipPip
  • 1,559 posts
  • LocationThe Hawkeye State

Posted 26 September 2013 - 08:32 PM

Same here Idaho, Cone 04, then Cone 06.