Posted 23 June 2013 - 08:30 AM

I want to put terra sig on greenware, bisque, then brush on and wipe off oxides or even black Lug underglaze to highlight texture. The one time I tried this, the oxide sat on top of the bisqued terra sig but would not soak in or even really attach to the pot. Suggestions, please?
Diane Puckett
Dry Ridge Pottery

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,355 posts
  • LocationRed Lodge, Montana

Posted 23 June 2013 - 10:32 AM

Sounds like your terra sig sealed. Maybe try bisque firing to a lower temp. But then you may not get the desired look of the terra sig.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,117 posts
  • LocationRaleigh, NC

Posted 24 June 2013 - 10:09 AM

You are fighting the nature of terra sig which is to give you a beautiful smooth sealed surface. A good terra sig leaves no little holes for your underglaze to grab onto which is why it doesn't. You will have to get your look a different way.
Chris Campbell Pottery
Contemporary Fine Colored Porcelain
http://ccpottery.com/

>TRY ... FAIL ... LEARN ... REPEAT"

" If a sufficient number of people are different, no one has to be normal "

Fredrick Bachman

#4 Diane Puckett

Diane Puckett

    Advanced Member

  • Members
  • PipPipPip
  • 398 posts
  • LocationAsheville, NC

Posted 24 June 2013 - 12:22 PM

I was afraid that was the situation but was hoping otherwise. Thanks, Marcia and Chris.