Im hoping for some suggestions on how to improve the colour intensity of coloured slips (without using a shiny glaze)
I want to achieve the (wet stone look) Ive always worked with sigilattas which im drawn to for there surface texture.
So im wanting to get a similar surface whilst using coloured stains?

#2 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,347 posts
  • LocationRed Lodge, Montana

Posted 09 May 2013 - 05:55 AM

What temperature are you using? What type of clay body?
What type of Glaze?What type of colorants for your slips?

All these are relevant.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#3 TJR

TJR

    Advanced Member

  • Members
  • PipPipPip
  • 1,821 posts
  • LocationWinnipeg,Manitoba,Canada

Posted 09 May 2013 - 08:07 AM

Im hoping for some suggestions on how to improve the colour intensity of coloured slips (without using a shiny glaze)
I want to achieve the (wet stone look) Ive always worked with sigilattas which im drawn to for there surface texture.
So im wanting to get a similar surface whilst using coloured stains?


You want to be looking up vitreous slips. Plenty of recipes for your relevant temp.I've used some, but not currently.
TJR.

#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,347 posts
  • LocationRed Lodge, Montana

Posted 09 May 2013 - 12:05 PM

so are you wanting to color terra sigs?
You can use mason stains for that. They can be added after the making of the sig.

Marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 larryinalabama

larryinalabama

    Member

  • Members
  • PipPip
  • 16 posts

Posted 09 May 2013 - 01:28 PM

If you used "colored slip " will it stain your molds?

#6 Diane Puckett

Diane Puckett

    Advanced Member

  • Members
  • PipPipPip
  • 398 posts
  • LocationAsheville, NC

Posted 09 May 2013 - 03:33 PM

I use mason stains in my colored slips. The biggest problem is the need to constantly stir them. If anyone has a suggestion to solve that issue, I would love to hear it.
Diane Puckett
Dry Ridge Pottery

#7 mitch72

mitch72

    Newbie

  • Members
  • Pip
  • 3 posts

Posted 09 May 2013 - 07:29 PM


Im hoping for some suggestions on how to improve the colour intensity of coloured slips (without using a shiny glaze)
I want to achieve the (wet stone look) Ive always worked with sigilattas which im drawn to for there surface texture.
So im wanting to get a similar surface whilst using coloured stains?


You want to be looking up vitreous slips. Plenty of recipes for your relevant temp.I've used some, but not currently.
TJR.


Yeah I thought vitreous slips might be the ticket. Do they give a different surface than spaying a thin layer of frit?

#8 mitch72

mitch72

    Newbie

  • Members
  • Pip
  • 3 posts

Posted 09 May 2013 - 07:31 PM

If you used "colored slip " will it stain your molds?



I dont mind seeing the traces of process