How to achieve this glaze effect

Recommended Posts

The glaze effect in the attached picture happened by happy accident where a 2nd glaze applied somewhat thickly to the top of the pot 'cracked' and the 1st glaze shows through. I like this and want more of the cracking next time. Any suggestions about technique or an additive to improve the chance that it will happen again?

 

This is fired to ^6 in electric kiln, and the glazes are Amaco PC Light Sepia over Deep Firebrick.

post-13888-136475261512_thumb.jpg

post-13888-136475261512_thumb.jpg

Share this post


Link to post
Share on other sites

The glaze effect in the attached picture happened by happy accident where a 2nd glaze applied somewhat thickly to the top of the pot 'cracked' and the 1st glaze shows through. I like this and want more of the cracking next time. Any suggestions about technique or an additive to improve the chance that it will happen again?

 

This is fired to ^6 in electric kiln, and the glazes are Amaco PC Light Sepia over Deep Firebrick.

 

 

If the bottom glaze is shiny and the top glaze is matt, you can get this affect.

TJR.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×