Posted 24 February 2013 - 06:29 AM

I have been using a matt transparent (commercial) glaze that I have been adding oxides etc to but would like to mix my own, does anyone have a recipe for a basic matt glaze? I am just starting out on the road to mixing my own glazes, but have been potting for many years.
Helz

#2 dawn523

dawn523

    Member

  • Members
  • PipPip
  • 13 posts
  • LocationLehigh Acres, Fl

Posted 24 February 2013 - 08:33 AM

What cone?