hi,

I have fired mistakenly the bisque on 1200.

How do i glaze?


Thank you,
Diana

#2 Lucille Oka

Lucille Oka

    Advanced Member

  • Members
  • PipPipPip
  • 756 posts
  • LocationCalifornia

Posted 06 February 2013 - 06:17 AM

1200 what centigrade or Fahrenheit?
John 3:16
"For God so loved the world that He gave His only begotten Son, that whosoever believeth in Him should not perish but have everlasting life".

#3 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,207 posts
  • LocationRed Lodge, Montana

Posted 06 February 2013 - 07:27 AM

1200 C would be about ^5. You may have vitrified the clay body depending on the type of clay you are using.
Some glazes may still cling to the surface. You can try heating the pots before trying to glaze. You can try adding a little gum to the glaze and spray it on..