Posted 04 January 2013 - 03:22 PM

One of the glazes posted in the Electric Kiln Firing download from Ceramic Arts Daily lists an ingredient as PV. I've racked my brain and looked through some chemical lists, but found nothing. What is PV? Thanks.

#2 Matt Oz

Matt Oz

    Advanced Member

  • Members
  • PipPipPip
  • 308 posts
  • LocationMichigan

Posted 04 January 2013 - 04:58 PM

My guess is Plastic Vitrox.