claclana Posted December 12, 2012 Report Share Posted December 12, 2012 Hello I had made a big tile and it's plaster mold, I didn't take it off and the clay is almost dry and do not know how to remove it, I wish not to hurt the plaster in the process, do you some suggestions? THANKS! Link to comment Share on other sites More sharing options...
minspargal Posted December 12, 2012 Report Share Posted December 12, 2012 Try spraying the clay with water to soften it up again, pull it off and start over. Link to comment Share on other sites More sharing options...
perkolator Posted December 12, 2012 Report Share Posted December 12, 2012 yeah, you can soften the clay up a bit and try to remove - but you'll have to dry it out longer to cure the mold before using. i recommend trying to use an air hose if you have access to air compressor - stream your air between the clay and plaster to try to release w/o damaging the plaster with tools. you can also use a damp sponge to remove clay from your plaster. Link to comment Share on other sites More sharing options...
claclana Posted December 12, 2012 Author Report Share Posted December 12, 2012 alright, I will try it! thank you! Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.