Dear All,

 

I did a quick refire last night of some work I wasn't happy with in a cone 6 firing. I lowered the firing range with these newly modified pieces to cone 5. Some new pieces I added to the mix appear underfired.

 

Can I now go with these sundry pieces (i.e., pieces I included in the cone 5 firing that I used to fill up the kiln) and that did not turn out great to cone 7?

 

I have never done this before.

 

My guess is that it is a crap shoot but that things should be okay if the initial glaze is compatible with a higher fire range.

 

Nelly

Share this post


Link to post
Share on other sites

Dear All,

 

I did a quick refire last night of some work I wasn't happy with in a cone 6 firing. I lowered the firing range with these newly modified pieces to cone 5. Some new pieces I added to the mix appear underfired.

 

Can I now go with these sundry pieces (i.e., pieces I included in the cone 5 firing that I used to fill up the kiln) and that did not turn out great to cone 7?

 

I have never done this before.

 

My guess is that it is a crap shoot but that things should be okay if the initial glaze is compatible with a higher fire range.

 

Nelly

 

 

 

Dear All,

 

Sorry about this post. I got my answer from my clay supplier. I will try to think a little more before I rapidly post.

 

This can be nuked.

 

Again, sorry about that.

 

Nelly

Share this post


Link to post
Share on other sites

Nelly, an annoying thing about a CAD post is that you can only delete the text, not the fact that you posted something. So if you want to get rid of the posted 'text', go to edit or full edit, highlight and delete it. Then click 'save modified post'. Your name date and time info will remain only. Do it before some one else replies and quotes your post.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.