If someone needs are large amount of sodium silicate / magic water
I wondered if Sugar Soap is a safe substitute to use instead of Terra Sigillata?

I checked out the ingredients in Selley's Sugar Soap powder and it has the exact ingredients
as the Magic Water terra sigillata recipe I discovered on the Ceramics Arts Daily forum.

Neutral salts 60% -
Sodium carbonate -30%
Sodium metasilicate,
pentahydrate -10%

Other ingredients determined
not to be hazardous

thanks!


#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,791 posts
  • LocationGrayslake, IL

Posted 01 June 2012 - 10:05 AM

Worth a try!

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users