Mitch Lyons, the man who came up with the clay Monoprint process spoke of using a charged material to hold on to the pigments. In this article he tells of how he spent years working on the process before coming up with Reemay landscaping fabric as his choice. In the article the author speaks of Lyons process and of using a clear water based spray sealant. If you google Mitch Lyons there are many videos describing his process plus on  Mitch Lyons website there is a DVD and a book from him on the topic.

 