Yas Posted May 22, 2018 Report Share Posted May 22, 2018 Until I finish the cone 10 porcelain that I still have, I need to continue to high fire in my electric kiln. Can someone suggest a firing schedule for cone 9 electric firing.....at least as a starting point? Thanks. Link to comment Share on other sites More sharing options...
neilestrick Posted May 22, 2018 Report Share Posted May 22, 2018 I would just use the Cone Fire mode on your controller, at medium speed. Those programs work great for 99% of what people fire. If you have a manual kiln, then 30-60 minutes each on low and medium, then high till it's done. Link to comment Share on other sites More sharing options...