How to make proper engobe mixture to clay roof tile(Max temp-900 Celcius)

Recommended Posts

Hi Malinda

i know from your previous post, you live in a region where laterite clay is used in the brick and roof industry. Laterite is an unique clay type with its own specific chemistry, not commonly found elsewhere. In fact, using it as an engobe over another clay, or using a different engobe over laterite simply will not work. The chemistry required to overcome laterite properties is complex. Wish I had better news for you.