can anyone tell me if they know , earthenware or stoneware, fired to the same temp., ^06, which will be most durable?



#2 Hobby Potter

Hobby Potter

    Newbie

  • Members
  • Pip
  • 8 posts

Posted 12 May 2010 - 09:07 AM

can anyone tell me if they know , earthenware or stoneware, fired to the same temp., ^06, which will be most durable?




Earthenware is usually most durable ^04, Stoneware at least ^6 I would assume the earthenware would be because it's closer to it maturation temperature.