Kaolinwasher Posted March 15, 2017 Report Share Posted March 15, 2017 i just got a bag of 325 mesh Custer feldspar. this march, I sent it on for a chemical analysis and we will see if its as discribed on there web site. the cost is ,27.50 for set up fee and about 5 bucks more for this and that and 30.65 per sample . Sent it in march 14 2017 i will let you all know the results. I got the bag from conntinental clay in Minneapolis MN 50 pound bag Link to comment Share on other sites More sharing options...
Dick White Posted March 15, 2017 Report Share Posted March 15, 2017 You da bomb, as they say in the 'hood. I'm really curious if/how far it has drifted since Ron Roy did this 5 years ago.Thanks for taking this on. Link to comment Share on other sites More sharing options...
Guest JBaymore Posted March 15, 2017 Report Share Posted March 15, 2017 Service to the field......... THANKS. best, ....................john Link to comment Share on other sites More sharing options...
Kaolinwasher Posted March 15, 2017 Author Report Share Posted March 15, 2017 i am also doing a porcelain test. with 30 custer and 20 flint in the 25 25 25 25 basic porcelain . For the flint I am using Sioux quartzite because it has some nice purple Iron in it . I want to see if it crazes, or shivers the glaze off. Link to comment Share on other sites More sharing options...
glazenerd Posted March 15, 2017 Report Share Posted March 15, 2017 Seems like a good time to start a pool... I put my money on a 7.95 potassium level. Link to comment Share on other sites More sharing options...