NancyChiassonDesigns Posted June 20, 2016 Report Share Posted June 20, 2016 I have a Gare Perfect Fire 2329D. Last 06 Bisque firing; programmed the Controller to ramp at 250 degrees F per hour (after firing to 250 degrees slowly). After 8 hours the temperature read 1180 degrees F and it was still ON. This Controller has a Soft Fire feature which I did not remember selecting. And, I don't fully understand and never have selected during bisque firings. When I reviewed the programmed instructions Soft Fire showed up so I select the "Down Arrow" and it stopped showing and the Kiln Shut Off. The buttons on the key pad have been getting sticky (?), it can take 3-4 presses to get the "Select" key to blink at the changes. I replaced all the elements and relays two years ago and am not near 100 firings. This is the most jam packed load of bisque I have ever fired! What should I troubleshoot first? Link to comment Share on other sites More sharing options...
NancyChiassonDesigns Posted June 24, 2016 Author Report Share Posted June 24, 2016 Just did a paper test and all the paper burned to ash in under 3 minutes. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.