tbaa Posted December 5, 2016 Author Report Share Posted December 5, 2016 My test tiles. Square ones fired in A Delhi studio where I went for a glaze course. The smaller ones below, fired in my test kiln. Clay from my own batch in both instances. Turquoise glaze is the lakeside studio recipe, mixed at the Delhi studio. two very different results. So thats what I'd like to keep working on - the firing schedule, and will see what the kiln's quirks are over time. Link to comment Share on other sites More sharing options...