Marcia Selsor Posted April 21, 2016 Report Share Posted April 21, 2016 First day of hands on working in Etorn with teapots by Corrie Bain and Laser Images Transfer with Tinua Wiard. E Torn os a fabulous studio with many resident artists of high professional experience. The image is made on a laser copier. Painter with the pigment mix. allowed to dry in minutes. the pigment sticks to the white surface and not the laser ink. Then the image is placed face down and on a damp tile and rubbed from the back with a spoon. Here are some images of laser copy transfer technique using stain and 10% alkaline glaze. Link to comment Share on other sites More sharing options...